FAQ
Ask the fastener question properly first.
20 answers across five categories. Short enough to cite, with a link to the standard, product family or article when you need the detail.
01
Selection & quotes
Are you a manufacturer or a sales company?
Integrated manufacturing and sales. We manufacture the fastener families that fit our lines, sell standard sizes from our warehouse, and keep one specification, inspection route and packing list across the order.
About the companyWhat is your minimum order quantity?
MOQ depends on the product, size, material and whether the item is a repeat line. We confirm it per line at quotation rather than quoting one number for the whole catalogue.
Send a quote requestWhat should I include in an RFQ?
The standard or drawing, thread and length, material and property class, finish, quantity, packing requirement and trade term. If a detail is missing, say so; we will flag it before quoting.
How quotes differWhy do quotes for the same drawing differ so much?
Usually the scope differs: steel grade, heat treatment, thread tolerance, coating thickness, inspection level, quantity, packing or trade term. A low price is not automatically wrong, but an unclear scope is a risk.
The seven cost variables02
Standards & drawings
Can you supply to DIN, ISO or GB standards?
Yes. We quote against the standard named on the order and confirm the drawing where dimensions or tolerances differ. Equivalent standards are a starting point, not a guarantee that every dimension is identical.
Standards guideWhat if the drawing and the standard number conflict?
Raise it before production. The drawing normally governs the part, but the standard may still define thread, property class or inspection. We mark the conflict on the quotation so both sides approve the same interpretation.
Standards libraryShould I choose DIN 933 or DIN 931?
DIN 933 is fully threaded; DIN 931 has a plain shank. Use full thread where the grip is short or adjustment is needed, and part thread where a plain shank is required at a shear plane. Confirm the thread length on the drawing.
DIN 933 detailWhat is a go/no-go thread gauge?
A go gauge should enter the full thread; a no-go gauge should not. It is a fast check of thread size and form, but it does not replace a full dimensional and mechanical inspection.
Inside a bolt batch03
Material & class
How do I choose between class 8.8 and 10.9?
Start from the load and the joint design. Class 10.9 gives higher strength but needs tighter control of material and heat treatment, and electroplated 10.9 parts need a de-embrittlement requirement.
Property class basicsHow do I choose between 304 and 316?
Start with chloride and moisture. 304 suits most indoor and general outdoor conditions. 316 contains molybdenum and is usually better for coastal, chemical and de-icing salt exposure. Crevices and passivation still matter.
304 on a coastCan stainless steel fasteners still rust?
Yes. Stainless steel relies on a passive film. Chlorides, crevices, dirt, iron contamination and scratches can break it and cause pitting or rust stains. Coastal and pool environments need cleaning and proper detailing.
Passivation and crevicesCan mill certificates and test reports travel with the goods?
When they are required, they should be agreed at quotation. We confirm which certificate or test report is needed, who issues it and whether it is batch-specific before the order is released.
Quality and inspection04
Finishes & corrosion
Zinc plating or hot-dip galvanizing?
Zinc plating is thinner and smoother, usually enough indoors or in light corrosion. Hot-dip galvanizing gives a thicker zinc layer for outdoor, wet or coastal work, but it affects thread fit and appearance.
Coating comparisonHow should coating thickness be written on the order?
Write the coating standard and the required class or minimum thickness, not just the colour. For electroplated parts, state whether de-embrittlement is required. Confirm the measurement method with the supplier.
Coating standardsCan electroplating cause hydrogen embrittlement?
High-strength steel parts can be at risk. The order should state the required de-embrittlement process and timing, especially for class 10.9 and above. Not every coating or part needs the same treatment.
Hydrogen riskWhat fasteners should I use on a coastal railing?
316 stainless is a common starting point, or hot-dip galvanized steel with a suitable coating system. Detail for drainage, isolate dissimilar metals and specify passivation. The environment, not the grade alone, decides.
Coastal selection05
Packing & export
Can you pack to our labels and shipping marks?
Yes, when the artwork and quantity are agreed before production. Send the label text, carton size, pallet requirement and shipping mark; we confirm what fits the line and what needs a separate run.
Talk to usWhat is the usual lead time?
It depends on the product, quantity, material, finish and whether tooling or a new coating route is needed. We give a lead time line by line in the quotation and confirm it again before production.
Request a scheduleDo you quote EXW, FOB or CIF?
Yes. The same goods can be quoted under different trade terms; the scope changes. Tell us the destination port and whether you want us to arrange freight and insurance, and we will quote the matching term.
Trade terms explainedWhich export documents do you provide?
Normally the commercial invoice and packing list, with the bill of lading from the forwarder. Certificates or inspection reports are added when agreed. Destination-specific requirements should be stated before shipment.
Export packingData & sources
What these answers are based on
Every answer here cites a registered standard or process claim. The same claim ID is shared with related articles, so the figure does not drift.
- DIN 933 is a hexagon head bolt with a full thread. DIN 933 · Standard / traceable
- DIN 931 is a hexagon head bolt with a partially threaded shank. DIN 931 · Standard / traceable
- Property class 8.8 has a nominal tensile strength of 800 MPa and a nominal yield strength of 640 MPa under ISO 898-1. ISO 898-1 · Standard / traceable
- Property class 10.9 has a nominal tensile strength of 1000 MPa and a nominal yield strength of 900 MPa under ISO 898-1. ISO 898-1 · Standard / traceable
- High-strength steel fasteners that are electroplated can be exposed to hydrogen embrittlement and should be specified with an appropriate de-embrittlement requirement. ISO 4042 / ASTM F1940 · Standard / traceable
- Type 304 stainless steel is typically about 18% chromium and 8% nickel. ASTM A276 / EN 10088 · Standard / traceable
- Type 316 stainless steel typically contains about 16–18% chromium, 10–14% nickel and 2–3% molybdenum. ASTM A276 / EN 10088 · Standard / traceable
- Stainless steel property class A2-70 has a nominal tensile strength of 700 MPa under ISO 3506-1. ISO 3506-1 · Standard / traceable
- Passivation is used to remove free iron and restore the passive film on stainless steel; ASTM A967 and ISO 16048 are common references. ASTM A967 / ISO 16048 · Standard / traceable
- When stainless steel is coupled to carbon steel in a wet environment, galvanic corrosion can accelerate corrosion of the carbon steel side. Corrosion engineering fundamentals · Standard / traceable
- ISO 4042 is a standard for electroplated coatings on fasteners. ISO 4042 · Standard / traceable
- ISO 1461 is a standard for hot-dip galvanized coatings on fabricated iron and steel articles. ISO 1461 · Standard / traceable
Still have a question?
Send the drawing or the question. We will answer directly.
Standard, material, size, quantity and service environment — send what you have.